Standard Specification for Martensitic Stainless Steel Bars for High-Temperature Service
STANDARD published on 1.3.2025
Designation standards: ASTM A565/A565M-10(2025)
Publication date standards: 1.3.2025
The number of pages: 4
Approximate weight : 12 g (0.03 lbs)
Country: American technical standard
Category: Technical standards ASTM
This guide covers standard specification for hot-finished and cold-finished martensitic chromium steel bars for high-temperature service. The mechanical properties shall be developed by suitable heat treatment, as indicated for each alloy. The steel shall conform to the required chemical composition for carbon, manganese, phosphorus, sulfur, silicon, chromium, nickel, molybdenum, vanadium, tungsten, nitrogen, aluminum, columbium, and copper. The microstructure shall not contain more than 5% delta-ferrite after full heat treatment. The material shall conform to the required mechanical properties such as tensile strength, yield strength, elongation, impact strength, and Brinell hardness. The material shall also undergo stress rupture testing using a combination test bar.
Keywords:
martensitic stainless steel, stainless steel bars, stainless steel billets, stainless steel forgings, temperature service applications—high,, ICS Number Code 77.140.60 (Steel bars and rods),77.140.85 (Iron and steel forgings)