Standard Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperatures
STANDARD published on 1.9.2012
Designation standards: ASTM A608/A608M-12
Note: WITHDRAWN
Publication date standards: 1.9.2012
The number of pages: 6
Approximate weight : 18 g (0.04 lbs)
Country: American technical standard
Category: Technical standards ASTM
Keywords:
alloy, centrifugal casting, high temperatures, pressure containing parts, steel tube, temperature service applications, ICS Number Code 23.040.10 (Iron and steel pipes), 23.040.40 (Metal fittings)