Aerospace series - Chloroprene rubber (CR) - Heat resistance - Hardness 60 IRHD.
STANDARD published on 1.6.2012
Designation standards: DIN EN 2837:2012-06
Publication date standards: 1.6.2012
The number of pages: 17
Approximate weight : 51 g (0.11 lbs)
Country: German technical standard
Category: Technical standards DIN
Luft- und Raumfahrt - Chloropren-Elastomere (CR) - Wärmebeständig - Härte 60 IRHD.