We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.
Standard Specification for Alloy and Structural Alloy Steel, Sheet and Strip, Hot-Rolled and Cold-Rolled
Translate name
STANDARD published on 1.9.2021
Designation standards: ASTM A506-16(2021)
Publication date standards: 1.9.2021
SKU: NS-1036725
The number of pages: 4
Approximate weight : 12 g (0.03 lbs)
Country: American technical standard
Category: Technical standards ASTM
This specification covers the standard for hot-rolled and cold-rolled alloy and structural alloy-steel sheet and strip. The material shall be furnished in several conditions: heat treatments such as hot-rolling and cold rolling; surface conditions; and edges, as specified herein, in coils or cut lengths. Heat analysis shall be performed on the material and shall conform to the required chemical compositions for carbon, manganese, phosphorus, sulfur, silicon, copper, nickel, chromium, molybdenum, and vanadium. Materials in the annealed, normalized, or normalized-and-tempered condition shall be capable of meeting the longitudinal bend test requirements. Two tension tests and two hardness tests shall be made from coupons obtained from each heat (cast) and heat treatment lot.
Keywords:
alloy steel sheet, alloy steel strip, cold-rolled alloy steel, hot-rolled alloy steel, standard alloy steel, structural alloy steel,, ICS Number Code 77.140.50 (Flat steel products and semi-products)
1. Scope | ||||
1.1?This specification covers hot-rolled and cold-rolled alloy and structural alloy-steel sheet and strip. Alloy steel is furnished to chemical composition requirements and is intended primarily for general or miscellaneous use where bending and moderate forming is a requirement. Structural alloy steel is furnished to chemical composition requirements and to specific mechanical property requirements which may include tension tests, hardness tests, or other commonly accepted mechanical tests. 1.2?If material of a higher degree of uniformity of internal soundness and freedom from surface imperfections is required, reference should be made to Specification A507. 1.3?Alloy and structural alloy-steel sheet and strip are not produced to internal cleanliness requirements. Normally surface imperfections are not objectionable, and a good finish is not a prime requirement. 1.4?The formability of structural alloy steel decreases with increasing yield strength or hardness. Therefore, product design in relation to the mechanical properties of the grade used must be considered. 1.5?The material covered by this specification may be furnished in several conditions: heat treatments, surface conditions, and edges, as specified herein, in coils or cut lengths. 1.6?The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. 1.7?This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee. |
||||
2. Referenced Documents | ||||
|
Do you want to make sure you use only the valid technical standards?
We can offer you a solution which will provide you a monthly overview concerning the updating of standards which you use.
Would you like to know more? Look at this page.
Latest update: 2024-12-22 (Number of items: 2 217 000)
© Copyright 2024 NORMSERVIS s.r.o.