Standard Test Method for Measurement of Internal Stress of Plated Metallic Coatings with the Spiral Contractometer
STANDARD published on 1.11.2010
Designation standards: ASTM B636-84(2010)
Note: WITHDRAWN
Publication date standards: 1.11.2010
SKU: NS-7513
The number of pages: 4
Approximate weight : 12 g (0.03 lbs)
Country: American technical standard
Category: Technical standards ASTM
Keywords:
internal stress test, metallic deposit, Electroplated coatings, Internal stress, Iron products (general)--electrodeposited coatings, Metallic coatings, Spiral contractometer, Steel--electrodeposited coatings, Stress--metallic materials, Stress cracking tests, ICS Number Code 25.220.40 (Metallic coatings)
Significance and Use |
The spiral contractometer, properly used, will give reproducible results (see 8.5) over a wide range of stress values. Internal stress limits with this method can be specified for use by both the purchaser and the producer of plated or electroformed parts. Plating with large tensile stresses will reduce the fatigue strength of a product made from high-strength steel. Maximum stress limits can be specified to minimize this. Other properties affected by stress include corrosion resistance, dimensional stability, cracking, and peeling. In control of electroforming solutions, the effects of stress are more widely recognized, and the control of stress is usually necessary to obtain a usable electroform. Internal stress limits can be determined and specified for production control. Internal stress values obtained by the spiral contractometer do not necessarily reflect the internal stress values found on a part plated in the same solution. Internal stress varies with many factors, such as coating thickness, preparation of substrate, current density, and temperature, as well as the solution composition. Closer correlation is achieved when the test conditions match those used to coat the part. |
1. Scope |
1.1 This test method covers the use of the spiral contractometer for measuring the internal stress of metallic coatings as produced from plating solutions on a helical cathode. The test method can be used with electrolytic and autocatalytic deposits. 1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
Do you want to make sure you use only the valid technical standards?
We can offer you a solution which will provide you a monthly overview concerning the updating of standards which you use.
Would you like to know more? Look at this page.
Latest update: 2024-11-22 (Number of items: 2 206 568)
© Copyright 2024 NORMSERVIS s.r.o.