We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.
Standard Test Method for Alkali-Solubility of Wools (Withdrawn 2022)
Automatically translated name:
Standard Test Method for Alkali-Solubility of Wools
STANDARD published on 1.1.2013
Designation standards: ASTM D1283-05(2013)
Note: WITHDRAWN
Publication date standards: 1.1.2013
SKU: NS-16869
The number of pages: 4
Approximate weight : 12 g (0.03 lbs)
Country: American technical standard
Category: Technical standards ASTM
Keywords:
Alkali-solubility and wool, ICS Number Code 59.060.10 (Natural fibres)
Significance and Use | ||||||||||||
5.1 Alkali-solubility is an indication of the degree of damage to wool resulting from certain chemical treatments, particularly when test results on the same wool, before such treatment, are available. 5.1.1 Undamaged scoured wool has typical alkali-solubility in the range of 9 to 15 %. Fine, undamaged wool normally will exhibit higher solubility than coarse wool, because of greater surface area per unit mass of fiber. 5.2 This test method is not recommended for use on wool known to have sustained alkali damage. 5.2.1 Alkali-damaged wool has had material solubilized that ordinarily would be included in the alkali-solubility test results. 5.3 Although results in one laboratory cannot usually be verified in another laboratory, this test method is considered satisfactory for acceptance testing because it has been used extensively in the trade for this purpose and because it is the only available method for assessing damage to wool by an alkali solubility procedure. Comparative tests as directed in 5.3.1 In case of a dispute arising from differences in reported test results when using Test Method D1283 for acceptance testing of commercial shipments, the purchaser and the supplier should conduct comparative tests to determine if there is a statistical bias between their laboratories. Competent statistical assistance is recommended for the investigation of bias. As a minimum, the two parties should take a group of test specimens which are as homogeneous as possible and which are from a lot of material of the type in question. The test specimens should then be randomly assigned in equal numbers to each laboratory for testing. The average result from the two laboratories should be compared using Student's t-test for unpaired data and an acceptable probability level chosen by the two parties before testing is begun. If a bias is found, either its cause must be found and corrected or the purchaser and the supplier must agree to interpret future test results in the light of the known bias. |
||||||||||||
1. Scope | ||||||||||||
1.1 This test method covers a chemical procedure for determination of the amount of wool substance soluble in alkali under standard conditions and is applicable to wool in scoured fiber form, or as fiber obtained from yarn or from woven or nonwoven fabric. 1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. 1.3 This standard does not
purport to address all of the safety concerns, if any, associated
with its use. It is the responsibility of the user of this standard
to establish appropriate safety and health practices and determine
the applicability of regulatory limitations prior to use.
|
||||||||||||
2. Referenced Documents | ||||||||||||
|
Do you want to make sure you use only the valid technical standards?
We can offer you a solution which will provide you a monthly overview concerning the updating of standards which you use.
Would you like to know more? Look at this page.
Latest update: 2024-11-22 (Number of items: 2 206 568)
© Copyright 2024 NORMSERVIS s.r.o.