We need your consent to use the individual data so that you can see information about your interests, among other things. Click "OK" to give your consent.
Adhesives for load-bearing timber structures - Test methods - Part 6: Determination of the minimum pressing time under referenced conditions
Translate name
STANDARD published on 1.7.2023
Designation standards: ČSN EN 302-6
Classification mark: 668531
Catalog number: 517003
Publication date standards: 1.7.2023
SKU: NS-1147147
The number of pages: 16
Approximate weight : 48 g (0.11 lbs)
Country: Czech technical standard
Category: Technical standards ČSN
This document specifies a method of determining the minimum pressing time for two glue line thicknesses, close contact glue line and thick glue line (between 0,3 mm and 8 mm), at three temperatures. It is applicable to adhesives used in load-bearing timber products.
This document is only intended for obtaining a reliable base of comparison of pressing time between adhesives. The method gives results that cannot be applied to the safe manufacture of timber structures without modifications for the influences of timber density/absorbency, moisture content, factory temperature and relative air humidity
Do you want to be sure about the validity of used regulations?
We offer you a solution so that you could use valid and updated legislative regulations.
Would you like to get more information? Look at this page.
Latest update: 2024-12-19 (Number of items: 2 216 019)